CPTC Thermistor:TPM Type
SMD CPTC Thermistor for Automotive Application
Soldering Recommendation
ꢀ
IR-Reflow Soldering Profile
Peak temp
Cooling
Preheating
255~260℃
60~150 sec
217℃
150~200℃
Tamb
3
℃
/sec
60~180 sec
6℃/sec
20~40
sec
3
℃
/sec
(max.)
(max.)
(max.
)
8 minutes max
Time
ꢀ
Reworking Conditions With Soldering Iron
Item
Conditions
360℃ (max.)
Temperature of Soldering Iron-tip
Diameter of Soldering Iron-tip
Soldering Time
Φ3mm (max.)
3 sec (max.)
Caution: Do not touch the component surface with soldering iron directly to
prevent it from damage.
THINKING ELECTRONIC INDUSTRIAL Co., LTD.
All specifications are subject to change without notice.