SAW FILTER
HDBF44A3Dc SIP5Dc
The specimen shall be passed through the reflow
furnace with the condition shown in the above
profile for 1 time.
The specimen shall be stored at standard
atmospheric conditions for 1h, after which the
measurement shall be made. Test board shall be
1.6 mm thick. Base material shall be glass fabric
base epoxy resin.
Solder ability Immerse the pins melt solder at 260℃+5/-0℃ More then 95% of
for 5 sec.
total area of the
pins should be
covered with solder
3.4 Mechanical Test
Items
Conditions
Specifications
Vibration
600-3300rpm amplitude 1.5mm
3 directions 2 H each
Drop
On maple plate from 1 m high 3 times
There shall be no
damage.
Lead pull
Lead bend
Pull with 1 kg force for 30 seconds
90o bending with 500g weigh 2 times
www.shoulder.cn Tel:0755-82916880 Fax:0755-82916881 E-mail:info@shoulder.cn
Page 7 of 10